Mechanical Properties Metric English Comments
Impact Test 21.9 J

@Temperature 22.8 °C
16.2 ft-lb

@Temperature 73.0 °F
Rheometric, 5mph, 1/2" diameter tup, 3" diameter ring
DuPont Bexloy® AXW507NC010 Modified Ionomer Resin  (discontinued **)
A modified ionomer resin engineered for injection molded exterior automotive applications.Availability: North AmericaInformation provided by DuPont.
Impact Test 21.9 J

@Temperature 22.8 °C
16.2 ft-lb

@Temperature 73.0 °F
Rheometric, 5mph, 1/2" diameter tup, 3" diameter ring
DuPont Bexloy® AXW504BK Modified Ionomer Resin  (discontinued **)
A modified ionomer resin engineered for injection molded exterior automotive applications.Availability: North AmericaInformation provided by DuPont.
Impact Test 21.9 J

@Temperature 22.8 °C
16.2 ft-lb

@Temperature 73.0 °F
Rheometric, 5mph, 1/2" diameter tup, 3" diameter ring
DuPont Bexloy® AXW602NC010 3% Glass Reinforced, Heat Stabilized Modified Ionomer Resin  (discontinued **)
A 3% glass reinforced, heat stabilized modified ionomer resin engineered for injection molded interior automotive applications.Availability: North AmericaInformation provided by DuPont.
Impact Test 22.0 J

@Temperature 0.000 °C
16.2 ft-lb

@Temperature 32.0 °F
Multi-Axial, Ductile; ASTM D3763
Flint Hills P9M6K-041A Specialty Impact Copolymer Polypropylene
Features: Good clarity and impact resistance. Product does not contain animal derived components.Applications: Injection molding - durable goodsInformation provided by Flint Hills Resources.
Impact Test 22.0 J

@Temperature 23.0 °C
16.2 ft-lb

@Temperature 73.4 °F
Instrumented Impact (0.5-in. dart, 3-in. clamp, 7.6 mph); Peak Energy; ASTM-D3763
Ineos ABS Lustran® LK197 ABS, Extrusion Grade
Lustran® ABS LK197 resin is a high-gloss, medium-impact extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It provides a superior balance between rigidity and impact strength, as well as e..
Impact Test 22.0 J

@Temperature -40.0 °C
16.2 ft-lb

@Temperature -40.0 °F
ASTM D3763
Diamond Polymers Centrex® 813 General Purpose Injection Molding Grade ASA/AES
Centrex 813 resin is a high-gloss, high-impact grade of ASA/AES, a blend of acrylonitrile-styrene-acrylate and acrylonitrile-ethylene-propylene styrene. This injection molding grade with a good bala..
Impact Test 22.0 J

@Temperature -30.0 °C
16.2 ft-lb

@Temperature -22.0 °F
Instrumented Dart Total Energy
Dow AIM® 4810 High Impact Styrenic Resin
AIM® 4810 advanced styrenic resin is designed to offer the processability of high impact polystyrene and the gloss and practical toughness of high gloss ABS. It can be processed at lower temperatur..
Impact Test 21.9 J

@Temperature 22.8 °C
16.2 ft-lb

@Temperature 73.0 °F
Rheometric, 5mph, 1/2" diameter tup, 3" diameter ring
DuPont Bexloy® AXW604BK 3% Glass Reinforced, Heat Stabilized Modified Ionomer Resin  (discontinued **)
A 3% glass reinforced, heat stabilized modified ionomer resin engineered for injection molded interior automotive applications.Availability: North AmericaInformation provided by DuPont.
Copyright © lookpolymers.com All Rights Reserved