Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 52.0 J @Temperature 23.0 °C |
38.4 ft-lb @Temperature 73.4 °F |
Instrumented Dart Total Energy |
Dow Prevail® 3150 ABS + Polyurethane PREVAIL® 3150 thermoplastic resin offers designers and manufacturers a combination of flexibility and low temperature toughness not previously available in an engineering thermoplastic and is used .. |