Material Notes:
PREVAIL® 3150 thermoplastic resin offers designers and manufacturers a combination of flexibility and low temperature toughness not previously available in an engineering thermoplastic and is used for applications ranging from flexible bumper fascias to sports equipment components. It is easy to process and is paintable without the need for a primer.Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
ASTM Data
Melt Density 0.970 g/cc
0.0350 lb/in³
Melt density
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
Melt Flow 11 g/10 min

@Load 2.16 kg,
Temperature 230 °C
11 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM Data
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 27.6 MPa
4000 psi
ASTM Data
Tensile Strength, Yield 24.1 MPa
3500 psi
ASTM Data
Elongation at Break 180 %
180 %
ASTM Data
Elongation at Yield 16 %
16 %
ISO Data
Tensile Modulus 0.745 GPa
108 ksi
ASTM Data
Izod Impact, Notched NB
NB
ASTM Data
3.74 J/cm

@Temperature -50.0 °C
7.01 ft-lb/in

@Temperature -58.0 °F
ASTM Data
Charpy Impact Unnotched NB
NB
ISO Data
NB
NB
ISO Data, Low Temp
Charpy Impact, Notched 4.15 J/cm²
19.8 ft-lb/in²
ISO Data, Low Temp
11.0 J/cm²
52.4 ft-lb/in²
ISO Data
Impact Test 52.0 J

@Temperature 23.0 °C
38.4 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
64.4 J

@Temperature -30.0 °C
47.5 ft-lb

@Temperature -22.0 °F
Instrumented Dart Total Energy
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 88.0 µm/m-°C

@Temperature 20.0 °C
48.9 µin/in-°F

@Temperature 68.0 °F
ASTM data
Specific Heat Capacity 1.54 J/g-°C
0.368 BTU/lb-°F
Thermal Conductivity 0.190 W/m-K
1.32 BTU-in/hr-ft²-°F
Deflection Temperature at 0.46 MPa (66 psi) 78.0 °C
172 °F
Unannealed; ASTM Data
93.0 °C
199 °F
Annealed; ASTM Data
Deflection Temperature at 1.8 MPa (264 psi) 63.0 °C
145 °F
Unannealed; ASTM Data
84.0 °C
183 °F
Annealed; ASTM Data
Vicat Softening Point 102 °C
216 °F
Optical Properties Metric English Comments
Gloss 72 %
72 %
Gardner Gloss, 60°
Copyright © lookpolymers.com All Rights Reserved