Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 39.0 J @Temperature -20.0 °C |
28.8 ft-lb @Temperature -4.00 °F |
Total Penetration Energy; ISO 6603-2 |
Borealis Borsoft™ SE410MO Polypropylene for Injection Molding Borsoft SE410MO is a specially designed modified relatively soft polypropylene heterophasic copolymer with medium melt flow intended for injection moldingBorsoft SE410MO is a tailor made grade desig.. |