Polymer Property : Impact Test = 45.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 45.0 J

@Temperature -20.0 °C
33.2 ft-lb

@Temperature -4.00 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Xenoy® 364 PBT
This data was supplied by SABIC-IP for the Americas region.
Impact Test 45.0 J

@Temperature 23.0 °C
33.2 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Valox® 364 PBT
Designed for outdoor telecommunications enclosure applications.This data was supplied by SABIC-IP for the Americas region.
Impact Test 45.0 J

@Temperature 23.0 °C
33.2 ft-lb

@Temperature 73.4 °F
ASTM D3763
Diamond Polymers Centrex® 810 Injection Molding Grade
Centrex 810 resin is a soft-flow, high-gloss, and medium-impact grade of ASA (acrylonitrile-styrene-acrylate). It is an injection molding grade with a good balance of physical properties, gloss and ..
Impact Test 45.0 J

@Thickness 4.00 mm
33.2 ft-lb

@Thickness 0.157 in
Multi-axial, total energy; ISO 6603-2
Azdel Plus C321B02N 32% Chopped Fiber Mat / PP Resin Matrix
AZDEL® C321B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a ..
Impact Test 45.0 J

@Thickness 4.00 mm
33.2 ft-lb

@Thickness 0.157 in
Multi-axial, total energy; ISO 6603-2
Azdel Plus R401B02N 40% Continuous Random Fiber Mat / PP Resin Matrix
AZDEL® R401B02N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a basic homogeneous fiber distribution. This m..
Impact Test 45.0 J

@Thickness 4.00 mm
33.2 ft-lb

@Thickness 0.157 in
Multi-axial, total energy; ISO 6603-2
Azdel Plus C401B02N 40% Chopped Fiber Mat / PP Resin Matrix
AZDEL® C401B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a ..