Mechanical Properties Metric English Comments
Impact Test 64.4 J

@Temperature -30.0 °C
47.5 ft-lb

@Temperature -22.0 °F
Instrumented Dart Total Energy
Dow Prevail® 3150 ABS + Polyurethane
PREVAIL® 3150 thermoplastic resin offers designers and manufacturers a combination of flexibility and low temperature toughness not previously available in an engineering thermoplastic and is used ..