Mechanical Properties Metric English Comments
Impact Test 7.00 J

@Temperature 23.0 °C
5.16 ft-lb

@Temperature 73.4 °F
Instrumented Impact Energy @ peak; ASTM D 3763
SABIC Innovative Plastics LNP Verton RV008ESV_GY7E072 PA 66
Preliminary data for 40% long glass fiber filled, single color pellet gray, PA66This data was supplied by SABIC-IP for the Americas region.
Impact Test 7.00 J

@Temperature 23.0 °C
5.16 ft-lb

@Temperature 73.4 °F
Multi-axial, at failure, measured on flat plaques; ASTM D3763
Azdel SuperLite® SL551000-100 PP Resin Matrix / 55% Glass Fiber (4 mm Molded Thickness)
AZDEL SuperLite® SL551000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Impact Test 7.00 J

@Temperature 23.0 °C
5.16 ft-lb

@Temperature 73.4 °F
Multi-axial, at max. load; ASTM D3763
Azdel SuperLite® SL551400-100 PP Resin Matrix / 55% Glass Fiber (8 mm Molded Thickness)
AZDEL SuperLite® SL551400-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Impact Test 7.00 J

@Temperature 23.0 °C
5.16 ft-lb

@Temperature 73.4 °F
Instrumented Impact Energy @ peak; ASTM D 3763
SABIC Innovative Plastics LNP Verton MV00ASUV_WH9D703 PP
Preliminary data for 50% Long fiber single color pellet filled PPThis data was supplied by SABIC-IP for the Americas region.
Impact Test 7.00 J

@Temperature 23.0 °C
5.16 ft-lb

@Temperature 73.4 °F
Instrumented Impact Energy @ peak; ASTM D 3763
SABIC Innovative Plastics LNP Verton RV006ESV_GY7E071 PA 66
Preliminary Data for 30% long glass fiber, single pellet color gray, PA66This data was supplied by SABIC-IP for the Americas region.