Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 9.00 J @Temperature -30.0 °C |
6.64 ft-lb @Temperature -22.0 °F |
Instrumented Impact; Total Energy; ASTM-D3763 |
Ineos ABS Lustran® 288 ABS, Injection Molding Grade Lustran® ABS 288 is a very high-flow injection molding grade of ABS (acrylonitrile butadiene styrene) with good impact strength and high gloss. It is intended for use in a wide range of applicati.. |
|||
Impact Test | 9.00 J @Thickness 4.00 mm |
6.64 ft-lb @Thickness 0.157 in |
Multi-axial, at max. load; ASTM D3763 |
Azdel Plus C321-B01 32% Chopped Fiber Mat / PP Resin Matrix AZDEL® C321-B01 is a glass mat thermoplastic laminate based upon a random oriented chopped fiber mat contained within a polypropylene resin matrix. This composite material features high flow prope.. |