Mechanical Properties Metric English Comments
100% Modulus 0.00131 GPa
0.190 ksi
ASTM D3574E
Mearthane Durethaneâ„¢ M DM-650A Foam Polyurethane
MDI backbone: ester.Shore 00 Hardness: 95Summary: Durethane M is a flexible, microcellular, open cell and closed cell urethane foam. Because it is mechanically mixed, the cell size is uniform. Dur..
100% Modulus 0.00131 GPa
0.190 ksi
Momentive Performance Materials LVG342 Low Volatile Silicone Adhesive, Mixed, White
LVG342 low volatile silicone adhesive is a two component, thixotropic silicone adhesive that cures very quickly at elevated temperatures to a durable elastomer. LV342 was specifically developed for..
100% Modulus 0.00131 GPa
0.190 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 40 PHR Non-Black, Precipitated Calcium Carbonate
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
100% Modulus 0.00131 GPa
0.190 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 40 PHR Non-Black, Precipitated Calcium Carbonate
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Copyright © lookpolymers.com All Rights Reserved