Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Mearthane Durethaneâ„¢ M DM-650A Foam Polyurethane

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane Foam, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer Mearthane Products Corporation (MPC)
Trade Name Durethane™ M
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mearthane Durethaneâ„¢ M DM-650A Foam Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MDI backbone: ester.Shore 00 Hardness: 95Summary: Durethane M is a flexible, microcellular, open cell and closed cell urethane foam. Because it is mechanically mixed, the cell size is uniform. Durethane M is very economical, and has excellent resistance to compression set. It can be formulated to form an integral skin.Applications: The compression set resistance of Durethane M makes it an effective material for applications with repeated compression cycles, such as actuator pads on postal meters and idler belts.Conductivity: All Durethane elastomers can be formulated to be electrically conductive, for applications involving electrostatic dissipation (ESD). Mearthane's proprietary conductivity process does not comprise the material performance specification of the urethane.Information provided by Mearthane Products Corporation.
Physical Properties Metric English Comments
Density 0.800 g/cc
0.0289 lb/in³
ASTM D3574A
Mechanical Properties Metric English Comments
Hardness, Shore A 50
50
ASTM D2240
Tensile Strength, Ultimate 79.3 MPa
11500 psi
ASTM D3574E
Elongation at Break 625 %
625 %
ASTM 3457E
100% Modulus 0.00131 GPa
0.190 ksi
ASTM D3574E
200% Modulus 0.00210 GPa
0.305 ksi
ASTM D3574E
300% Modulus 0.00314 GPa
0.455 ksi
ASTM D3574E
Compressive Yield Strength 0.480 MPa
69.6 psi
at 10% deflection; ASTM D3574C
0.720 MPa
104 psi
at 20% deflection; ASTM D3574C
1.03 MPa
149 psi
at 30% deflection; ASTM D3574C
Resilience 40
40
Bashore Rebound; ASTM 2632D
Tear Strength Test 130
130
lb; Die C; ASTM 3457F