Polymer Property : 100% Modulus = 0.00152 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00152 GPa
0.220 ksi
ASTM D412
Huntsman IROGRAN® PS455-203 TPU-Polyester
Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers
100% Modulus 0.00152 GPa
0.220 ksi
ASTM D412
SK Chemicals SKYTHANE® T850A Polyester Based, Low Hardness Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
100% Modulus 0.00152 GPa
0.220 ksi
ASTM D412
Teknor Apex UNIPRENE® 7100-45 Thermoplastic Elastomer
Information provided by Teknor Apex Company
100% Modulus 0.00152 GPa
0.220 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Non-Black, Translink 555
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
100% Modulus 0.00152 GPa
0.220 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Non-Black, Translink 555
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..