Polymer Property : 100% Modulus = 0.00193 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00193 GPa
0.280 ksi
ASTM D412
Huntsman KRYSTALFLEX® PE 429 Polyurethane Optical Aliphatic Film
Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers
100% Modulus 0.00193 GPa
0.280 ksi
Injection molded plaques, Die C, Machine Direction; ASTM D412
Kraton® G2705 GU (SEBS) Compound
Description: Kraton G2705 GU-N is an easy processing material designed for applications where FDA regulations are required. The material exhibits high resilience, low compression set, and good punct..
100% Modulus 0.00193 GPa
0.280 ksi
ASTM D412; ISO 37
Advanced Polymer Alloys Alcryn® 2250 UT Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..