Mechanical Properties Metric English Comments
100% Modulus 0.00207 GPa
0.300 ksi
ASTM D412
S&E Specialty Polymers TufTech™ GA-1052-55 PVC Compound
Application: A 105°C scuff, oil and flame resistant high flow molding compound designed for grommets.Information provided by S&E Specialty Polymers
100% Modulus 0.00207 GPa
0.300 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR Iceberg Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00207 GPa
0.300 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR Suprex Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00207 GPa
0.300 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Hardness 63A
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00207 GPa
0.300 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Hardness 75A
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00207 GPa
0.300 ksi
ASTM D412
Huntsman KRYSTALFLEX® PE 399 Polyurethane Optical Aliphatic Film
Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers
100% Modulus 0.00207 GPa
0.300 ksi
ASTM D412
Teknor Apex UNIPRENE® 7010-55 Thermoplastic Elastomer
Information provided by Teknor Apex Company
100% Modulus 0.00207 GPa
0.300 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Hardness 63A
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00207 GPa
0.300 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Hardness 75A
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00207 GPa
0.300 ksi
ASTM D412
Lubrizol Estane® ALR E72A Thermoplastic Polyurethane
Type: Estane® ALR E72A is a clear aliphatic thermoplastic polyurethane (TPU).Features: Non-yellowing with good mechanical properties.Available in AmericasInformation Provided by The Lubrizol Corpor..
100% Modulus 0.00207 GPa
0.300 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR Suprex Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00207 GPa
0.300 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR N990 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00207 GPa
0.300 ksi
ASTM D412
Lubrizol Estane® ALR PC73A Thermoplastic Polyurethane
Type: Estane® ALR PC73A is a polycarbonate diol based thermoplastic polyurethane (TPU).Features: Hydrolytically stable, very durableAvailable in Americas, Europe, Middle East, Africa, India and Asi..
100% Modulus 0.00207 GPa
0.300 ksi
cured 7 mins @ 150°C
ACC QSil 550R QSI Quantum Silicones Silicone Potting Material
QSil 550Ris a 100% silicone solids elastomer designed for electronic potting applications. The two-component system offers a hard, thermally conductive, low modulus material that is readily repairab..
100% Modulus 0.00207 GPa
0.300 ksi
cured 20 mins @ 150°C
ACC QSil 550SB QSI Quantum Silicones Self-Priming Silicone Potting Material
QSil 550SB is a 100% silicone solids elastomer designed for electronic potting applications. The two-component system offers a hard, thermally conductive, low modulus material that is readily repair..
100% Modulus 0.00207 GPa
0.300 ksi
ASTM D638
Colorite Polymers 5002 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
100% Modulus 0.00207 GPa
0.300 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR N339 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00207 GPa
0.300 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR N339 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00207 GPa
0.300 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR Iceberg Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00207 GPa
0.300 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR N990 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..