Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : 100% Modulus = 0.00234 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00234 GPa
0.340 ksi
ASTM D412
Lubrizol Estane® AG 4950 Thermoplastic Polyurethane
Type: Estane® AG 4950 is a polyether based aliphatic thermoplastic polyurethane (TPU) specifically formulated to be used as an adhesive interlayer in transparencies for electronic displays, aerospa..
100% Modulus 0.00234 GPa
0.339 ksi
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, Hardness 70A
Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed ..
100% Modulus 0.00234 GPa
0.340 ksi
ASTM D 412
CPT C-Flex® R70-003 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
100% Modulus 0.00234 GPa
0.340 ksi
Press Cure 7 minutes @ 177°C, Post Cure 24 hours @ 260°C
3M Dyneon™ FT 2430 Fluoroelastomer
3M™ Dyneon™ Fluoroelastomer FT 2430 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul..
100% Modulus 0.00234 GPa
0.339 ksi
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, Hardness 70A
Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed ..