Mechanical Properties Metric English Comments
100% Modulus 0.00259 GPa
0.375 ksi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, 350ºF Cure Temperature
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
100% Modulus 0.00259 GPa
0.375 ksi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, 350ºF Cure Temperature
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
100% Modulus 0.00259 GPa
0.376 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 40 PHR Non-Black, Translink 555
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
100% Modulus 0.00259 GPa
0.375 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR Iceberg Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00259 GPa
0.375 ksi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 20 PHR Mistron Vapor Filler
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
100% Modulus 0.00259 GPa
0.375 ksi
Press Cure 7 minutes @ 177°C, Post Cure 24 hours @ 260°C
3M Dyneon™ FE 5730 Fluoroelastomer
Composition: Ter-polymer of vinylidene fluoride, hexafluoropropylene and tetrafluoroethyleneLower fluorine version of FE 5830QProcess targets: extrusion onlyProprietary incorporated cure technologyP..
100% Modulus 0.00259 GPa
0.375 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR Iceberg Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00259 GPa
0.376 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 40 PHR Non-Black, Translink 555
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
100% Modulus 0.00259 GPa
0.375 ksi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 20 PHR Mistron Vapor Filler
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Copyright © lookpolymers.com All Rights Reserved