Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00330 GPa | 0.479 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR Talc-Mistron Vapor MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00330 GPa | 0.479 ksi | DIN 53504 |
Huntsman IROGRAN® A 70 E 4675 Polyester-Based TPU-High Performance Grade Introduction: IROGRAN A 70 E 4675 is a softener free thermoplastic special-polyester-polyurethane for injection molding applications. Additional characteristics of the product are very short cycle t.. |
|||
100% Modulus | 0.00330 GPa | 0.479 ksi | Cecilia 20 aged 168 hrs at 175°C |
DuPont Vamac® DP Sartomer 350 Coagent Test Compound Vamac® DP is an ethylene acrylic dipolymer elastomer. Its general performance characteristics are similar to those of the Vamac® terpolymers, including:Good oil and chemical resistanceHigh temper.. |
|||
100% Modulus | 0.00330 GPa | 0.479 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR Talc-Mistron Vapor MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00330 GPa | 0.478 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Carbon Black, N-330 (HAF) Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
100% Modulus | 0.00330 GPa | 0.479 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4570 Radiator/Heater Hose FormulationNordel® IP 4570 |
|||
100% Modulus | 0.00330 GPa | 0.479 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4640 General Purpose Compound FormulationNordel® IP 4640 |
|||
100% Modulus | 0.00330 GPa | 0.478 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Carbon Black, N-330 (HAF) Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |