Mechanical Properties Metric English Comments
100% Modulus 0.00330 GPa
0.479 ksi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR Talc-Mistron Vapor
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
100% Modulus 0.00330 GPa
0.479 ksi
DIN 53504
Huntsman IROGRAN® A 70 E 4675 Polyester-Based TPU-High Performance Grade
Introduction: IROGRAN A 70 E 4675 is a softener free thermoplastic special-polyester-polyurethane for injection molding applications. Additional characteristics of the product are very short cycle t..
100% Modulus 0.00330 GPa
0.479 ksi
Cecilia 20 aged 168 hrs at 175°C
DuPont Vamac® DP Sartomer 350 Coagent Test Compound
Vamac® DP is an ethylene acrylic dipolymer elastomer. Its general performance characteristics are similar to those of the Vamac® terpolymers, including:Good oil and chemical resistanceHigh temper..
100% Modulus 0.00330 GPa
0.479 ksi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR Talc-Mistron Vapor
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
100% Modulus 0.00330 GPa
0.479 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
Dow Nordel® IP 4570 Radiator/Heater Hose
FormulationNordel® IP 4570
100% Modulus 0.00330 GPa
0.479 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
Dow Nordel® IP 4640 General Purpose Compound
FormulationNordel® IP 4640