100% Modulus 0.00380 GPa
0.551 ksi
ISO/R527
Polykemi AB POLYelast TPE Z800 SHF Thermoplastic Elastomer, SEBS-based
Information provided by Polykemi AB
100% Modulus 0.00380 GPa
0.551 ksi
ISO/R527
Polykemi AB POLYelast TPE Z800 Thermoplastic Elastomer, SEBS-based
Information provided by Polykemi AB
100% Modulus 0.00380 GPa
0.551 ksi
TPE-0153 (ASTM D 412)
ExxonMobil Santoprene® 521-70 Thermoplastic Rubber  (discontinued **)
A black thermoplastic elastomer designed for glazing and sealing applications with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonat..
100% Modulus 0.00380 GPa
0.551 ksi
Formulation Example
TSE Industries Millathane® 66 Millable Polyurethane Rubber
Millathane 66 is a peroxide-curable polyurethane rubber for the production of oil, fuel and chemical resistant parts which require excellent low and high temperature performance and high mechanical ..
100% Modulus 0.00380 GPa
0.551 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
Dow Nordel® IP 4760P Compound
FormulationNordel® IP 4760P
100% Modulus 0.00380 GPa
0.551 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
Dow Nordel® IP 4770P Dense Extruded Profile
FormulationNordel® IP 4770P
100% Modulus 0.00380 GPa
0.551 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
Dow Nordel® IP 4770R Dense Extruded Profile
FormulationNordel® IP 4770R
100% Modulus 0.00380 GPa
0.551 ksi
Formulation Example
TSE Industries Millathane® 66 Millable Polyurethane Rubber
Millathane 66 is a peroxide-curable polyurethane rubber for the production of oil, fuel and chemical resistant parts which require excellent low and high temperature performance and high mechanical ..
100% Modulus 0.00380 GPa
0.551 ksi
ASTM D412; ASTM D638
Lubrizol Estane® 58280 Thermoplastic Polyurethane
Type: Estane® 58280 is a polyether-type thermoplastic polyurethane (TPU) compound.Features: High resiliency compound, with unique physical properties such as low tensile and compression set, high r..
100% Modulus 0.00380 GPa
0.551 ksi
ISO 37
AlphaGary Evoprene™ HP 3730 High Performance Thermoplastic Elastomer
Evoprene™ HP is a hydrogenated styrene block copolymer based thermoplastic elastomer. Specially formulated for applications requiring high strength and excellent abrasion resistance, Evoprene™ HP..