Material Notes:
FormulationNordel® IP 4760P
Physical Properties Metric English Comments
Mooney Viscosity 55

@Temperature 100 °C
55

@Temperature 212 °F
ML 1 + 4
Mechanical Properties Metric English Comments
Hardness, Shore A 69
69
Vulcanizate, Press cured, TC95 +3min at 160°C
Tensile Strength, Ultimate 14.4 MPa
2090 psi
Vulcanizate, Press cured, TC95 +3min at 160°C
Modulus of Elasticity 0.00130 GPa
0.189 ksi
25% Modulus, Vulcanizate, Press cured, TC95 +3min at 160°C
50% Modulus 0.00200 GPa
0.290 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
100% Modulus 0.00380 GPa
0.551 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
200% Modulus 0.00800 GPa
1.16 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
Tear Strength 26.3 kN/m
150 pli
Die C, Vulcanizate, Press cured, TC95 +3min at 160°C
Compression Set 35 %

@Temperature 100 °C
35 %

@Temperature 212 °F
22 hr