Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00420 GPa | 0.609 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR N220 (ISAF) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00420 GPa | 0.609 ksi | ASTM D412 |
Elastocon TPE Technologies Elastocon® CLR75 Thermoplastic Elastomer Elastocon® CLR75 is a transparent thermoplastic elastomer that has been developed for applications that require oil/plasticizer free, non-blooming high strength properties and a tactile surface fin.. |
|||
100% Modulus | 0.00420 GPa | 0.609 ksi | ASTM D412 |
Elastocon TPE Technologies Elastocon® STK56PA-B Thermoplastic Elastomer Elastocon® STK56PA-B black thermoplastic elastomer has been developed for applications that require soft rubber-like properties and a good surface finish. Elastocon® STK56PA-B is well suited for .. |
|||
100% Modulus | 0.00420 GPa | 0.609 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR N220 (ISAF) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00420 GPa | 0.609 ksi | Cured 7 min at 177°C and Post Cured 2 hr at 232°C |
DuPont Performance Polymers VTR 8655 (GBL-S) Peroxide Cured Fluoroelastomer (FKM)
(discontinued **) FormulationVTR 8655 |