Polymer Property : 100% Modulus = 0.609 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00420 GPa
0.609 ksi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR N220 (ISAF) Filler
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
100% Modulus 0.00420 GPa
0.609 ksi
ASTM D412
Elastocon TPE Technologies Elastocon® CLR75 Thermoplastic Elastomer
Elastocon® CLR75 is a transparent thermoplastic elastomer that has been developed for applications that require oil/plasticizer free, non-blooming high strength properties and a tactile surface fin..
100% Modulus 0.00420 GPa
0.609 ksi
ASTM D412
Elastocon TPE Technologies Elastocon® STK56PA-B Thermoplastic Elastomer
Elastocon® STK56PA-B black thermoplastic elastomer has been developed for applications that require soft rubber-like properties and a good surface finish. Elastocon® STK56PA-B is well suited for ..
100% Modulus 0.00420 GPa
0.609 ksi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR N220 (ISAF) Filler
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
100% Modulus 0.00420 GPa
0.609 ksi
Cured 7 min at 177°C and Post Cured 2 hr at 232°C
DuPont Performance Polymers VTR 8655 (GBL-S) Peroxide Cured Fluoroelastomer (FKM)  (discontinued **)
FormulationVTR 8655