Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00540 GPa | 0.783 ksi | Value at 50°C is 1.8 MPa; ASTM D412-80 |
DuPont Performance Polymers Hypalon® 45 Chlorosulfonated Polyethylene Rubber, Uncured Carbon Black Filled Compound
& Carbon black compound with 100 parts Hypalon; 100 parts carbon black; 4 parts magnesia; and 1.5 parts propylene glycol. Physical property data below (except mooney viscosity) are for uncured film. .. |
|||
100% Modulus | 0.00540 GPa | 0.783 ksi | ASTM D412 |
Mearthane Durethaneâ„¢ S DS-290A Solid Polyurethane Elastomer TDI backbone: ester.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, .. |
|||
100% Modulus | 0.00540 GPa | 0.783 ksi | |
Taiwan PU Corporation TPU-E85 General Grade, Extrusion Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Extrusion MoldingInformation provided by Taiwan PU Corporation. |
|||
100% Modulus | 0.00540 GPa | 0.783 ksi | |
Taiwan PU Corporation TPU-EH80 High Hydrolysis Resistance, Extrusion Molding Polyether Base TPU Thermoplastic Polyurethane (TPU), High Hydrolysis Resistance, Polyether Base, Extrusion MoldingInformation provided by Taiwan PU Corporation. |
|||
100% Modulus | 0.00540 GPa | 0.783 ksi | |
Taiwan PU Corporation TPUI-E80 General Grade, Injection Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
100% Modulus | 0.00540 GPa | 0.783 ksi | |
Taiwan PU Corporation TPUI-G85 High Wear Resistance, Injection Molding Polycaprolactone Base TPU Thermoplastic Polyurethane (TPU), High Wear Resistance, Polycaprolactone Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
100% Modulus | 0.00540 GPa | 0.783 ksi | DIN 53504 |
Lubrizol ESTANE® 58300 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
100% Modulus | 0.00540 GPa | 0.783 ksi | DIN 53504 |
Lubrizol ESTANE® 5714F1 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
100% Modulus | 0.00540 GPa | 0.783 ksi | |
Colorite Polymers Vinylbond 95-950-70 PVC Compound Description: Vinylbond 95-950 series compounds are flexible PVC alloys which are formulated specifically for the window market industry. These compounds offer excellent bonding characteristics to ri.. |
|||
100% Modulus | 0.00540 GPa | 0.783 ksi | Cured 7 min at 177°C and Post Cured 2 hr at 232°C |
DuPont Performance Polymers VTR 8600 (GF-S) Peroxide Cured Fluoroelastomer (FKM)
(discontinued **) FormulationVTR-8600 |