Mechanical Properties Metric English Comments
100% Modulus 0.00655 GPa
0.950 ksi
ASTM D412
Teknor Apex UNIPRENE® 7100-87 Thermoplastic Elastomer
Information provided by Teknor Apex Company
100% Modulus 0.00655 GPa
0.950 ksi
ASTM D412
Teknor Apex Uniprene® 87A Polyvinyl Chloride, Flexible
Features: High Elastic RecoveryInformation Provided by Teknor Apex
100% Modulus 0.00655 GPa
0.950 ksi
heat aged 70 hours at 300ºF
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 60 PHR N330 (HAF) Black
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
100% Modulus 0.00655 GPa
0.950 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR N339 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00655 GPa
0.950 ksi
Colorite Polymers Self Frosting™ 7011SF Vinyl Compound
Description: Colorite has developed a family of vinyl compounds to satisfy the needs of those who need a smooth, low gloss, low friction surface for the products that they produce. Historically, thi..
100% Modulus 0.00655 GPa
0.950 ksi
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
3M Dyneon™ FE 5522 Fluoroelastomer
3M™ Dyneon™ Fluoroelastomer FE 5522 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul..
100% Modulus 0.00655 GPa
0.950 ksi
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
3M Dyneon™ FE 5620Q Fluoroelastomer
3M™ Dyneon™ Fluoroelastomer FE 5620Q can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formu..
100% Modulus 0.00655 GPa
0.950 ksi
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
3M Dyneon™ FE 5621 Fluoroelastomer
3M™ Dyneon™ Fluoroelastomer FE 5621 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul..
100% Modulus 0.00655 GPa
0.950 ksi
ASTM D-638
Axiall 2010 Wire & Cable Flexible PVC
General purpose insulation and jacketing compound recommended for 75°C applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.00655 GPa
0.950 ksi
ASTM D-638
Axiall 10752 Wire & Cable Flexible PVC
General purpose 75C jacket compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.00655 GPa
0.950 ksi
heat aged 70 hours at 300ºF
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 60 PHR N330 (HAF) Black
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
100% Modulus 0.00655 GPa
0.950 ksi
Colorite Polymers 7011 Clear Extrusion Vinyl Compound
Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for the extrusion of various components for the production of devices. The vinyl components used in pre..
100% Modulus 0.00655 GPa
0.950 ksi
Colorite Polymers 7012 Clear Injection Molding Vinyl Compound
Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for injection molding of various components such as drip chambers, connectors, valves, etc. The vinyl c..
100% Modulus 0.00655 GPa
0.950 ksi
Colorite Polymers Vinylbond 95-950-80 PVC Compound
Description: Vinylbond 95-950 series compounds are flexible PVC alloys which are formulated specifically for the window market industry. These compounds offer excellent bonding characteristics to ri..
100% Modulus 0.00655 GPa
0.950 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR N339 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Copyright © lookpolymers.com All Rights Reserved