Material Notes:
3M™ Dyneon™ Fluoroelastomer FE 5621 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formulations. The “dry” ingredients should be blended before adding to the masticated gum. For best results, Dyneon FE 5621 should be banded on the mill several minutes prior to adding the blended dry ingredients. Once mixed, the compounded stocks have good scorch resistance and storage stabilityComposition: Di-polymer of vinylidene fluoride and hexafluoropropyleneLow shrink version of FE 5620QProcess targets: injection and transfer molding, extrusion and calenderingImproved scorch resistance at high molding temperaturesProprietary incorporated cure technologyExcellent mold release-can be used in automated injection molding equipmentImproved cure technology resulting in more consistent part size from successive molding cyclesClean runningInformation provided by Dyneon, A 3M Company
Physical Properties Metric English Comments
Specific Gravity 1.80 g/cc
1.80 g/cc
Mooney Viscosity 23

@Temperature 121 °C
23

@Temperature 250 °F
ML1+10
Mechanical Properties Metric English Comments
Hardness, Shore A 77
77
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C; ASTM D2240
Tensile Strength at Break 15.4 MPa
2240 psi
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
Elongation at Break 195 %
195 %
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
100% Modulus 0.00655 GPa
0.950 ksi
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
Compression Set 13 %
13 %
Aged 70 hours @ 200°C; ASTM D395
Thermal Properties Metric English Comments
Transformation Temperature -18.0 °C
-0.400 °F
TR10; ASTM D1329
Component Elements Properties Metric English Comments
Fluorine, F 65.9 %
65.9 %
Descriptive Properties Value Comments
Color Opaque Off-White
MH, Maximum Torque 21.9 inch-lb
100 cpm, 0.5° Arc, 6 Minutes @ 177°C
ML, Minimum Torque 0.7 inch-lb
100 cpm, 0.5° Arc, 6 Minutes @ 177°C
Solubility Ketones and Esters
t`50, Time to 50% cure 2.6 minutes
100 cpm, 0.5° Arc, 6 Minutes @ 177°C
t`90 - Time to 90% cure 3.7 minutes
100 cpm, 0.5° Arc, 6 Minutes @ 177°C
ts2 - Time to 2 in-lb rise from min 2.3 minutes
100 cpm, 0.5° Arc, 6 Minutes @ 177°C