Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.007701 GPa | 1.117 ksi | |
Seals Eastern Perflas® 9295 Perfluorinated Rubber Perfluoro rubber for high-temperature, aggressive chemical service. Perflas 9295® seals offer high temperature service and are resistant to aggressive chemicals. They are a thermally stable, pe.. |