Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00880 GPa | 1.28 ksi | ASTM D412 |
Precision Polymer Engineering Perlast® G75S Perfluoroelastomer Perlast® G75S has been specifically developed to cope with a wide range of process media, potent active pharmaceutical ingredients (APIs) and aggressive cleaning agents, being especially suited to .. |
|||
100% Modulus | 0.00880 GPa | 1.28 ksi | |
Taiwan PU Corporation TPUI-L90 Low Temperature Resistance, Injection Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), Low Temperature Resistance, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
100% Modulus | 0.00880 GPa | 1.28 ksi | Heat aged 2 weeks at 175°C |
DuPont Vamac® DP HVA-2 Coagent Test Compound Vamac® DP is an ethylene acrylic dipolymer elastomer. Its general performance characteristics are similar to those of the Vamac® terpolymers, including:Good oil and chemical resistanceHigh temper.. |
|||
100% Modulus | 0.00880 GPa | 1.28 ksi | ASTM D412 |
C.O.I.M. LARIPUR® LPR9020 Standard Adipate Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
100% Modulus | 0.00880 GPa | 1.28 ksi | Cured 7 min at 177°C and Post Cured 16 hr at 200°C |
DuPont Performance Polymers VTR 8710 (ETP-600S) Peroxide Cured Fluoroelastomer (FKM) Formulation
(discontinue FormulationViton® Extreme™ ETP-600S |