Polymer Property : 100% Modulus = 1.28 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00880 GPa
1.28 ksi
ASTM D412
Precision Polymer Engineering Perlast® G75S Perfluoroelastomer
Perlast® G75S has been specifically developed to cope with a wide range of process media, potent active pharmaceutical ingredients (APIs) and aggressive cleaning agents, being especially suited to ..
100% Modulus 0.00880 GPa
1.28 ksi
Taiwan PU Corporation TPUI-L90 Low Temperature Resistance, Injection Molding Polyester Base TPU
Thermoplastic Polyurethane (TPU), Low Temperature Resistance, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation.
100% Modulus 0.00883 GPa
1.28 ksi
Taiwan Sheen Soon Sheenthane® A9513H TPU for Ink
Thermoplastic polyurethane elastomer for inkAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen printing, and spray applicati..
100% Modulus 0.00882 GPa
1.28 ksi
JIS K6301
Stellarchem FP-860 TPE Compound
Product description : This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric poly..
100% Modulus 0.00880 GPa
1.28 ksi
Heat aged 2 weeks at 175°C
DuPont Vamac® DP HVA-2 Coagent Test Compound
Vamac® DP is an ethylene acrylic dipolymer elastomer. Its general performance characteristics are similar to those of the Vamac® terpolymers, including:Good oil and chemical resistanceHigh temper..
100% Modulus 0.00880 GPa
1.28 ksi
ASTM D412
C.O.I.M. LARIPUR® LPR9020 Standard Adipate Ester Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..
100% Modulus 0.00881 GPa
1.28 ksi
C.O.I.M. PLAXTER® P 70 Polymeric Plasticizer
Description: Formulated with PVC, it is used in the field of conveyor belt manufacturing as well as in the field of synthetic leathers.Information provided by P.A.T. Products, Inc.
100% Modulus 0.00880 GPa
1.28 ksi
Cured 7 min at 177°C and Post Cured 16 hr at 200°C
DuPont Performance Polymers VTR 8710 (ETP-600S) Peroxide Cured Fluoroelastomer (FKM) Formulation  (discontinue
FormulationViton® Extreme™ ETP-600S