Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : 100% Modulus = 0.00896 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00896 GPa
1.30 ksi
ASTM D412
S&E Specialty Polymers G-3085E PVC
Application: General purpose PVC material with good low temperature properties designed for T-Molding extrusion applicationsInformation provided by S&E Specialty Polymers
100% Modulus 0.00896 GPa
1.30 ksi
Dow Pellethane® 2103-90AEF Polyurethane Elastomer, Ether Based  (discontinued **)
PELLETHANE® 2103-90AEF elastomer is a polytetramethylene glycol ether based polyurethane elastomer, featuring superior resilience, low temperature properties, excellent hydrolytic stability, and re..
100% Modulus 0.00896 GPa
1.30 ksi
Dow Pellethane® 2103-90AEN Polyurethane Elastomer, Ether Based  (discontinued **)
PELLETHANE® 2103-90AEN is a polytetramethylene glycol ether based polyurethane elastomer featuring superior resilience, low temperature properties, excellent hydrolytic stability, and resistance to..
100% Modulus 0.00896 GPa
1.30 ksi
ASTM D412
Lubrizol Advanced Materials PEARLTHANE® 16N92 Thermoplastic Polyurethane Elastomer  (discontinued **)
PEARLTHANE® 16N92 is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent mechanical properties and excellent hydrolysis resistance. It can b..
100% Modulus 0.00896 GPa
1.30 ksi
25 mil film; ASTM D412
Huntsman IROGRAN® A 95 P 5003 TPU-Polyether
IROGRAN® A 95 P 5003 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications.Information provided by Alliance Polymers
100% Modulus 0.00896 GPa
1.30 ksi
Spartech M60480 General Purpose PVC
First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B..
100% Modulus 0.00896 GPa
1.30 ksi
ASTM D412
SK Chemicals SKYTHANE® R190A Polyether Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
100% Modulus 0.00896 GPa
1.30 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 90A, Black Sulfur Cure
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
100% Modulus 0.00896 GPa
1.30 ksi
ASTM D638
Colorite Polymers 7502 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
100% Modulus 0.00896 GPa
1.30 ksi
ASTM D638
Colorite Polymers 8200FR General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
100% Modulus 0.00896 GPa
1.30 ksi
ASTM D-638
Axiall EX 3114B Plenum Flexible PVC
Non-lead stabilized CAT 3 jacket recommended for hybrid constructions. Also recommended for 25+ pair counts.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.00896 GPa
1.30 ksi
ASTM D-638
Axiall EX1188A Wire & Cable Flexible PVC
UL 360 jacket compound. 80°C air; 60°C oil.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.00896 GPa
1.30 ksi
ASTM D412
ACC EP RSP-AL EPI Engineered Polymers Aromatic Silicone Polyurea
EP RSP-AL, Aromatic Silicone Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Polyurea. This increases UV resistance without sacrificing physical properties. EP RSP-AL..
100% Modulus 0.00896 GPa
1.30 ksi
ASTM D-638
Axiall 38552 Wire & Cable Flexible PVC
General purpose insulating and jacketing compound for 105°C AWM and SPT applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.00896 GPa
1.30 ksi
ASTM D-638
Axiall 38601 Coax & Telecom Flexible PVC
CATV and general purpose jacket. UL recognized for 720 hour sunlight resistance in all colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.00896 GPa
1.30 ksi
ASTM D-638
Axiall 830 Wire & Cable Flexible PVC
TW insulation. UL recognized for TW and Oil resistant II.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.00896 GPa
1.30 ksi
ASTM D-638
Axiall 8803 Moldings & Extrusions Flexible PVC
Microbe resistant extrusion and molding compound designed for use in weatherstrips, screen spline and flexible gaskets. Good UV resistance.Information provided by Georgia GulfGeorgia Gulf became Ax..
100% Modulus 0.00896 GPa
1.30 ksi
ASTM D-638
Axiall 8900 Moldings & Extrusions Flexible PVC
General purpose extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.00896 GPa
1.30 ksi
ASTM D412
ACC EP RSP EPI Engineered Polymers Silicone Polyurea
EP RSP Silicone Polyurea, “Powered by Reactamine®Technology”, is a two component 100% solid Polyurea with superior performance in industrial applications. EP RSP displays extremely fast cure time..
100% Modulus 0.00896 GPa
1.30 ksi
ASTM D-638
Axiall 2192 Wire & Cable Flexible PVC
Non-lead stabilized SJTO, SJTOO oil resistant flexible cord jacket. UL recognized for 720 hour sunlight resistance in all colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corpo..
100% Modulus 0.00896 GPa
1.30 ksi
ASTM D638
Colorite Polymers 8007SF General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
100% Modulus 0.00896 GPa
1.30 ksi
ASTM D-638
Axiall 8843 Moldings & Extrusions Flexible PVC
General purpose, non-lead stabilized extrusion compound. Well suited for 80°C rated automotive tubing.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.00896 GPa
1.30 ksi
ISO 37
PolyOne Elastamax XL 0254-15 TPU-Based Thermoplastic Elastomer  (discontinued **)
This is a urethane based thermoplastic elastomer specially lubricated for auto suspension bushings. Physical Form: Pellets. Standard Color: Natural.Information provided by M. A. Hanna. M. A. Hann..
100% Modulus 0.00896 GPa
1.30 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 90A, Black Sulfur Cure
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
100% Modulus 0.00896 GPa
1.30 ksi
Dow Pellethane® 2354-45D Polyurethane Elastomer, Polyester Polycaprolactone Based  (discontinued **)
PELLETHANE® 2354-45D elastomer is a polyester polycaprolactone based polyurethane elastomer used in automotive applications. It allows fast molding, and once molded can be painted with polyurethane..
Copyright © lookpolymers.com All Rights Reserved