Axiall 38552 Wire & Cable Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 38552 Wire & Cable Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General purpose insulating and jacketing compound for 105°C AWM and SPT applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 76 - 82
76 - 82
delayed; ASTM D-2240
83 - 89
83 - 89
ASTM D-2240
Tensile Strength, Yield 15.9 MPa
2300 psi
ASTM D-638
Elongation at Yield 280 %
280 %
Air Aging: 168 hours @ 136°C; 30 mil slabs; UL 1581
350 %
350 %
ASTM D-638
100% Modulus 0.00896 GPa
1.30 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -35.0 °C
-31.0 °F
ASTM D-746
Oxygen Index 24.5 %
24.5 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 182 °C
360 °F