Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00979 GPa | 1.42 ksi | |
Taiwan Sheen Soon Sheenthane® A9030 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
100% Modulus | 0.00979 GPa | 1.42 ksi | |
Taiwan Sheen Soon Sheenthane® A9519UK Film Grade Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for blown filmInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
100% Modulus | 0.00979 GPa | 1.42 ksi | |
Taiwan Sheen Soon Sheenthane® A9600R Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |