Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00980 GPa | 1.42 ksi | |
Taiwan PU Corporation TPUI-E95 General Grade, Injection Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
100% Modulus | 0.00980 GPa | 1.42 ksi | |
Taiwan PU Corporation TPUI-H95 High Hydrolysis Resistance, Injection Molding Polyether Base TPU Thermoplastic Polyurethane (TPU), High Hydrolysis Resistance, Polyether Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
100% Modulus | 0.00980 GPa | 1.42 ksi | |
Taiwan PU Corporation TPUI-T85 Transparent Grade, Injection Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), Transparent Grade, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
100% Modulus | 0.00979 GPa | 1.42 ksi | |
Taiwan Sheen Soon Sheenthane® A9030 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
100% Modulus | 0.00979 GPa | 1.42 ksi | |
Taiwan Sheen Soon Sheenthane® A9519UK Film Grade Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for blown filmInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
100% Modulus | 0.00979 GPa | 1.42 ksi | |
Taiwan Sheen Soon Sheenthane® A9600R Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
100% Modulus | 0.00980 GPa | 1.42 ksi | JIS K6301 |
Stellarchem GP-860 TPE Compound Product description : This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric poly.. |
|||
100% Modulus | 0.00981 GPa | 1.42 ksi | JIS-A-5756 |
Denka VINYKON M7300 PVC, M grade for soft injection molding A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
100% Modulus | 0.00981 GPa | 1.42 ksi | JIS-A-5756 |
Denka VINYKON W3050 PVC, W grade for equipment cords, for heat resistance A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |