Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.0121 GPa | 1.75 ksi | ASTM D412 |
Teknor Apex UNIPRENE® 7010-50D Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
100% Modulus | 0.0121 GPa | 1.75 ksi | Press cure 15 Minutes @ 188°C, Post Cure 16 Hours @ 250°C |
3M Dyneon™ PFE 4131TZ High Temperature Perfluoroelastomer 3M™ Dyneon™ PFE 4131TZ is an incorporated cure high temperature perfluoroelastomer (HT PFE). It is designed to meet the challenges of higher temperature applications. It is classified as FFKM per .. |
|||
100% Modulus | 0.0121 GPa | 1.75 ksi | ASTM D-638 |
Axiall 15880-02 Wire & Cable Flexible PVC TW, 60C oil. 80C Class 43 insulation. Oil resistant I. 300 hour sunlight resistant.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0121 GPa | 1.75 ksi | ASTM D-638 |
Axiall 15881 Wire & Cable Flexible PVC 80C general purpose. 300 hour sunlight resistant.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0121 GPa | 1.75 ksi | ASTM D-638 |
Axiall 17881 Wire & Cable Flexible PVC THW insulation compound. UL recognized component for TW, THW insulation.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0121 GPa | 1.75 ksi | ASTM D-638 |
Axiall 17883 Wire & Cable Flexible PVC UV resistant, 90C insulation compound with good low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0121 GPa | 1.75 ksi | ASTM D-638 |
Axiall 19881 Wire & Cable Flexible PVC 105°C rated clear compound recommended for 30 mils and larger.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0121 GPa | 1.75 ksi | Plasticizer conc. in vinyl film 50 phr; ASTM D638 |
BASF Palatinol® 11P-E (DUP) Linear Phthalate Formula: C30H50O4Description: Palatinol® 11P-E plasticizer is a linear phthalate ester based on a predominately linear C11 alcohol. Palatinol 11P-E exhibits very low volatility and good processing .. |
|||
100% Modulus | 0.0121 GPa | 1.75 ksi | ASTM D-638 |
Axiall 19880 Wire & Cable Flexible PVC 105°C rated, 30 mil and larger, clear compound recommended for VW-1 applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0121 GPa | 1.75 ksi | ASTM D-638 |
Axiall 22882 Coax & Telecom Flexible PVC Flexible flame retardant jacket compound suitable for "patch cable" constructions over HDPE primaries.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0121 GPa | 1.75 ksi | ASTM D-638 |
Axiall 22883 Coax & Telecom Flexible PVC Flexible, matte-finish, flame retardant jacket compound suitable for "patch cable" constructions over HDPE primaries.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 201.. |
|||
100% Modulus | 0.0121 GPa | 1.75 ksi | ASTM D-638 |
Axiall 34431 Wire & Cable Flexible PVC TW insulation. UL recognized for TW, Oil resistant I and VW-1.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0121 GPa | 1.75 ksi | |
Dow Pellethane® 2354-55D Polyurethane Elastomer, Polyester Polycaprolactone Based
(discontinued **) PELLETHANE® 2354-55D is elastomer is a polyester polycaprolactone based polyurethane elastomer used in automotive applications. It allows fast molding, and once molded can be painted with polyureth.. |
|||
100% Modulus | 0.0121 GPa | 1.75 ksi | ASTM D412 |
Dow PELLETHANE® 2355-55DE Polyurethane Elastomer, Polyester Polyadipate Based
(discontinued **) Description: PELLETHANE® 2355-55DE polyester polyadipate based polyurethane elastomer has excellent oil and chemical resistance. Applications include: Film, Sheet, Tubing, Recreation and sporting e.. |