Material Notes:
Flexible flame retardant jacket compound suitable for "patch cable" constructions over HDPE primaries.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.40 - 1.44 g/cc
1.40 - 1.44 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 85 - 91
85 - 91
delayed; ASTM D-2240
Tensile Strength, Yield 17.2 MPa
2500 psi
ASTM D-638
Elongation at Yield 230.1 %
230.1 %
Air Aging: 240 hours @ 100°C; 30 mil slabs; UL 1581
300 %
300 %
ASTM D-638
100% Modulus 0.0121 GPa
1.75 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -30.0 °C
-22.0 °F
ASTM D-746
Oxygen Index 32.5 %
32.5 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 185 °C
365 °F