Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.0159 GPa | 2.30 ksi | ASTM D412 |
S&E Specialty Polymers TufTech™ GA-5748C-01 PVC Compound Application: RoHS compliant, PVC based compound suitable for THHN, THWN, applications.Information provided by S&E Specialty Polymers |
|||
100% Modulus | 0.0159 GPa | 2.30 ksi | ASTM D412 |
SK Chemicals SKYTHANE® L194A Polycaprolactone Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
100% Modulus | 0.0159 GPa | 2.31 ksi | DIN 53504 |
Lubrizol ESTANE® T4086 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
100% Modulus | 0.0159 GPa | 2.30 ksi | ASTM D638 |
Colorite Polymers 9002 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.0159 GPa | 2.30 ksi | ASTM D638 |
Colorite Polymers 9234 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.0159 GPa | 2.30 ksi | ASTM D638 |
Colorite Polymers 93-636B General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.0159 GPa | 2.30 ksi | ASTM D-638 |
Axiall 19450 Wire & Cable Flexible PVC 105°C rated insulation compound with very good migration and oil resistance. Recommended for toner resistant applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation.. |
|||
100% Modulus | 0.0159 GPa | 2.30 ksi | ASTM D-638 |
Axiall 19473 Wire & Cable Flexible PVC Non-lead stabilized, 105°C insulation compound recommended for a minimum wall thickness of 10 mils. Designed to meet the performance criteria of military spec. MIL-W-16878D.Information provided by.. |
|||
100% Modulus | 0.0159 GPa | 2.31 ksi | ASTM D412 |
Lubrizol Pellethane® 2363-55DE Thermoplastic Polyurethane Elastomer Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |