100% Modulus 0.00241 GPa
0.350 ksi
heat aged 70 hours at 300ºF
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR N330 (HAF) Black
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
100% Modulus 0.00241 GPa
0.350 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR N220 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00241 GPa
0.350 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR N650 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00241 GPa
0.350 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR Iceberg Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00241 GPa
0.350 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR Suprex Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00241 GPa
0.350 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR Suprex Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00241 GPa
0.350 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Hardness 66A
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00241 GPa
0.350 ksi
ASTM D412
Mearthane Durethaneâ„¢ S DS-370A Solid Polyurethane Elastomer
TDI backbone: ether.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, ..
100% Modulus 0.00241 GPa
0.350 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Hardness 66A
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00241 GPa
0.350 ksi
heat aged 70 hours at 300ºF
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR N330 (HAF) Black
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
100% Modulus 0.00241 GPa
0.350 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR Iceberg Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00241 GPa
0.350 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR N990 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00241 GPa
0.350 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR Suprex Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00241 GPa
0.350 ksi
ASTM D638
Colorite Polymers 87-638A General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
100% Modulus 0.00241 GPa
0.350 ksi
ASTM D-638
Axiall 8602 Moldings & Extrusions Flexible PVC
A vinyl elastomer extrusion compound with rubber-like properties. Ideally suited for extruded profiles, tubings and co-extruded shapes.Information provided by Georgia GulfGeorgia Gulf became Axiall..
100% Modulus 0.00241 GPa
0.350 ksi
ASTM D-638
Axiall 8540 Moldings & Extrusions Flexible PVC
General purpose, flexible PVC compound recommended for extrusion or molding applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.00241 GPa
0.350 ksi
ASTM D-638
Axiall 8554 Moldings & Extrusions Flexible PVC
General purpose, jelly clear flexible PVC compound recommended for extrusion or molding applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.00241 GPa
0.350 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR N330 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00241 GPa
0.350 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR N990 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00241 GPa
0.350 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR Suprex Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00241 GPa
0.350 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR N220 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00241 GPa
0.350 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR N330 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00241 GPa
0.350 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR N650 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00241 GPa
0.350 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR Suprex Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00241 GPa
0.350 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR Suprex Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00241 GPa
0.350 ksi
ASTM D412-98
Saint-Gobain Fluran® F-5500-A Fluoroelastomer Tubing
Fluran® Severe Environment Tubing has the physical and chemical characteristics that make it ideal for severe environments, such as dry cleaning fluid lines and solvent recovery systems, where othe..