Mechanical Properties Metric English Comments
100% Modulus 0.00179 - 0.00269 GPa
0.260 - 0.390 ksi
ASTM D412
Huntsman KRYSTALFLEX® PE 399 Polyurethane Optical Aliphatic Film
Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers