Mechanical Properties Metric English Comments
100% Modulus 0.00343 GPa
0.498 ksi
Taiwan Sheen Soon Sheenthane® A7020 TPU for Ink
Thermoplastic polyurethane elastomer for ink. Hydrolysis resistance gradeAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen..
100% Modulus 0.00343 GPa
0.498 ksi
Taiwan Sheen Soon Sheenthane® A7710 TPU for Ink
Thermoplastic polyurethane elastomer for ink. Hydrolysis resistance gradeAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen..
100% Modulus 0.00343 GPa
0.498 ksi
Taiwan Sheen Soon Sheenthane® A7711 TPU for Ink
Thermoplastic polyurethane elastomer for ink. Hydrolysis resistance gradeAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen..
100% Modulus 0.00343 GPa
0.498 ksi
Taiwan Sheen Soon Sheenthane® A7810H TPU for Ink
Thermoplastic polyurethane elastomer for inkAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen printing, and spray applicati..
100% Modulus 0.00343 GPa
0.498 ksi
Taiwan Sheen Soon Sheenthane® A7810H TPU for Ink
Thermoplastic polyurethane elastomer for inkAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen printing, and spray applicati..
100% Modulus 0.00343 GPa
0.498 ksi
Taiwan Sheen Soon Sheenthane® A7810L TPU for Ink
Thermoplastic polyurethane elastomer for inkAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen printing, and spray applicati..
100% Modulus 0.00343 GPa
0.498 ksi
500 mm/min; ASTM D 412
Zylog Neoplast® 155 FT SWB Thermoplastic Vulcanizate
Neoplast 155 FT SWB is a soft, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding and Extrusion applications.RoHS Compliant,..
100% Modulus 0.00343 GPa
0.498 ksi
Parallel Flow; ASTM D412
Advanced Polymer Alloys DuraGrip™ 6165 TR Thermoplastic Elastomer
DuraGrip® DGR6165TR is a translucent thermoplastic elastomer (TPE) formulated for excellent elastic properties and enhanced adhesion to engineered thermoplastics using insert molding, co-injection ..