Material Notes:
Neoplast 155 FT SWB is a soft, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding and Extrusion applications.RoHS Compliant, UV StabilizedInformation provided by Zylog Plastalloys Pvt. Ltd.
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D 792
Mechanical Properties Metric English Comments
Hardness, Shore A 58
58
ASTM D 2240
60

@Treatment Temp. 150 °C,
Time 605000 sec
60

@Treatment Temp. 302 °F,
Time 168 hour
Heat Aging; ASTM D 2240/ASTM D 573
Tensile Strength, Ultimate 4.90 MPa
711 psi
500 mm/min; ASTM D 412
5.49 MPa

@Treatment Temp. 150 °C,
Time 605000 sec
797 psi

@Treatment Temp. 302 °F,
Time 168 hour
Heat Aging; ASTM D 412/ASTM D 573
Elongation at Break 250 %
250 %
500 mm/min; ASTM D 412
212 %

@Treatment Temp. 150 °C,
Time 605000 sec
212 %

@Treatment Temp. 302 °F,
Time 168 hour
Heat Aging; ASTM D 412/ASTM D 573
100% Modulus 0.00343 GPa
0.498 ksi
500 mm/min; ASTM D 412
Tear Strength 21.6 kN/m
123 pli
500 mm/min; ASTM D 624
Compression Set 32 %

@Temperature 70.0 °C,
Time 79200 sec
32 %

@Temperature 158 °F,
Time 22.0 hour
ASTM B 395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 125 °C
257 °F
Continuous; SAE J 2236
Brittleness Temperature -60.0 °C
-76.0 °F
ASTM D 746