Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00359 GPa | 0.520 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, 400ºF Cure Temperature MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
100% Modulus | 0.00359 GPa | 0.520 ksi | ASTM D412 |
SK Chemicals SKYTHANE® S175A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
100% Modulus | 0.00359 GPa | 0.520 ksi | ASTM D412 |
Teknor Apex UNIPRENE® 7010-73 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
100% Modulus | 0.00359 GPa | 0.520 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, 400ºF Cure Temperature MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
100% Modulus | 0.00359 GPa | 0.520 ksi | After 7 days at 257°F (125°C); ASTM D573; ISO 188 |
Advanced Polymer Alloys Alcryn® 2070 NC Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
100% Modulus | 0.00359 GPa | 0.520 ksi | ASTM D412; ISO 37 |
Advanced Polymer Alloys Alcryn® 2265 UT Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
100% Modulus | 0.00359 GPa | 0.520 ksi | Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C |
3M Dyneon™ FC 2122 Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FC 2122 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul.. |