Teknor Apex UNIPRENE® 7010-73 Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Teknor Apex Company
Trade Name UNIPRENE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex UNIPRENE® 7010-73 Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Teknor Apex Company
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc
0.960 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 73
73
5 seconds; ASTM D2240
Tensile Strength, Yield 6.55 MPa
950 psi
ASTM D412
Elongation at Break 380 %
380 %
ASTM D412
100% Modulus 0.00359 GPa
0.520 ksi
ASTM D412
Tear Strength 33.3 kN/m
190 pli
ASTM D624
Compression Set 28 %
28 %
23°C, 22 hr.; ASTM D395, Method B
52 %
52 %
100°C, 22 hr.; ASTM D395, Method B
Thermal Properties Metric English Comments
Brittleness Temperature <= -60.0 °C
<= -76.0 °F
ASTM D746