100% Modulus 0.006867 GPa
0.9960 ksi
JIS-K-6723
Denka REOMER G G5074 Thermoplastic Elastomer, For Extrusion
Essentially a thermoplastic elastomer with the characteristics of PVC resin and rubber, with excellent rubber-like elasticity. Offers excellent rubbery characteristics, such as permanent compressive..
100% Modulus 0.006867 GPa
0.9960 ksi
JIS-K-6723
Denka REOMER G G8070 Thermoplastic Elastomer, For Injection Molding
Essentially a thermoplastic elastomer with the characteristics of PVC resin and rubber, with excellent rubber-like elasticity. Offers excellent rubbery characteristics, such as permanent compressive..