Mechanical Properties Metric English Comments
100% Modulus 0.006998 GPa
1.015 ksi
ASTM D412
Lubrizol Advanced Materials PEARLTHANE® 16N87 Thermoplastic Polyurethane Elastomer  (discontinued **)
PEARLTHANE® D16N87 is a polyether-based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, offering adequate hardness with superior hydrolysis resistance and improved e..
100% Modulus 0.006998 GPa
1.015 ksi
ASTM D412
Lubrizol Advanced Materials Pearlthane® 12H92E Thermoplastic Polyurethane Elastomer
Pearlthane® 12H92E is a special polyester-based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent processability and excellent low temperature performance..