Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.0114 GPa | 1.65 ksi | ASTM D412 |
Precision Polymer Engineering Perlast® G81H Perfluoroelastomer Special, pure white compound with PTFE blended for improved dynamic performance. Has excellent chemical resistance, steam resistance and mechanical properties. Extremely low outgassing properties. .. |
|||
100% Modulus | 0.0114 GPa | 1.65 ksi | DIN 53504 |
Huntsman IROGRAN® A 92 K 5031 TPU-High Temperature Performance Polycaprolactone and ether based. Good processability and compression set. Excellent resistance to high temperatures, water, grease, and oils.. Used in seals, wheels, and rollers.Information prov.. |
|||
100% Modulus | 0.0114 GPa | 1.65 ksi | ASTM D412 |
Mearthane Durethaneâ„¢ S DS-450D Solid Polyurethane Elastomer TDI backbone: ester.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, .. |
|||
100% Modulus | 0.0114 GPa | 1.65 ksi | ASTM D412 |
Mearthane Durethaneâ„¢ S DS-695A Solid Polyurethane Elastomer MDI backbone: ester.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, .. |
|||
100% Modulus | 0.0114 GPa | 1.65 ksi | ASTM D-638 |
Axiall 9115A Wire & Cable Flexible PVC Low cost tray cable jacket.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0114 GPa | 1.65 ksi | ASTM D-638 |
Axiall 10850 Wire & Cable Flexible PVC Non-metallic conduit. 3/4" and smaller.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0114 GPa | 1.65 ksi | ASTM D-638 |
Axiall 35061 Coax & Telecom Flexible PVC CMR jacket over PVC or flame retardant PE insulation with excellent low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0114 GPa | 1.65 ksi | ASTM D-638 |
Axiall 384FR Wire & Cable Flexible PVC Highly flame retardant jacketing compound recommended for direct burial applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0114 GPa | 1.65 ksi | ASTM D-638 |
Axiall 39012 Coax & Telecom Flexible PVC Flame retardant CATV and general purpose jacket. UL recognized for sunlight resistance in all colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0114 GPa | 1.65 ksi | ISO 37 |
Lubrizol ESTANE® 58212 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |