Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.0245 GPa | 3.55 ksi | |
Taiwan Sheen Soon Sheenthane® D6010 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
100% Modulus | 0.0245 GPa | 3.55 ksi | |
Taiwan Sheen Soon Sheenthane® D6010E Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
100% Modulus | 0.0245 GPa | 3.55 ksi | |
Taiwan Sheen Soon Sheenthane® D6320E Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
100% Modulus | 0.0245 GPa | 3.55 ksi | |
Taiwan Sheen Soon Sheenthane® D6610 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
100% Modulus | 0.0245 GPa | 3.55 ksi | JIS K6301 |
Stellarchem GP-785A TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
100% Modulus | 0.0245 GPa | 3.55 ksi | JIS K6301 |
Stellarchem GP-980 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |