Polymer Property : Tensile Impact Strength = 163 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Impact Strength 145 - 163 kJ/m²
69.0 - 77.6 ft-lb/in²
Average value: 154 kJ/m² Grade Count:4
Overview of materials for Medium Density Polyethylene (MDPE), Rotational Molded
This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Rotational Molded". Each property range of values reported is minimu..