Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 145 - 163 kJ/m² | 69.0 - 77.6 ft-lb/in² | Average value: 154 kJ/m² Grade Count:4 |
Overview of materials for Medium Density Polyethylene (MDPE), Rotational Molded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Rotational Molded". Each property range of values reported is minimu.. |