Mechanical Properties Metric English Comments
Tensile Impact Strength 502 kJ/m²
239 ft-lb/in²
23°C; ASTM D-1822
ExxonMobil Escorene® LD-781 High EVA Compounding Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 33% vinyl acetate copolymer for specialty compounding applications. The resin provides excellent stress cracking and flexibility, and allows outs..