Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 502 kJ/m² | 239 ft-lb/in² | 23°C; ASTM D-1822 |
ExxonMobil Escorene® LD-781 High EVA Compounding Resin