Polymer Property : Tensile Impact Strength = 252 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Impact Strength 252 kJ/m²
120 ft-lb/in²
ASTM D1822
ExxonMobil HDPE HD 9856B High Density Polyethylene Resin
Product Description: HD 9856B is a HDPE blow molding resin designed for high performance packaging applications. Containers made from HD 9856B exhibit a unique combination of stiffness and environme..
Tensile Impact Strength 252 kJ/m²
120 ft-lb/in²
ASTM D1822
ExxonMobil Paxon™ BA50-100 Blow Molding Resin
Product Description: BA50-100 is a high molecular weight, high density polyethylene copolymer. This resin has superior stress crack resistance, high impact strength and good rigidity.Availability: ..
Tensile Impact Strength 252 kJ/m²
120 ft-lb/in²
Molded and tested in accordance with ASTM D4976; ASTM D1822, Type S
Dow DNDA-7340 NT 7 Linear Low Density Polyethylene Resin
DOW DNDA-7340 NT 7 LLDPE resin is well-suited for use in blow molding applications such as small, squeezable bottles, as well as, extruded flexible hoses and tubing. DOW DMDA-7340 NT 7 resin is als..
Tensile Impact Strength 252 kJ/m²
120 ft-lb/in²
Molded and tested in accordance with ASTM D4976; ASTM D1822, Type S
Dow UNIVAL™ DMDC-6145 NT 7 High Density Polyethylene Resin (HDPE)
Excellent parison melt strength / low sag Good extrudability / process-ability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDC-6145 NT 7 provides good parison stability, which contribu..
Tensile Impact Strength 252 kJ/m²
120 ft-lb/in²
ASTM D1822
ExxonMobil HD 9856B Blow Molding Resin
Product Description: HD 9856B is a HDPE blow molding resin designed for high performance packaging applications. Containers made from HD 9856B exhibit a unique combination of stiffness and environme..
Tensile Impact Strength 252 kJ/m²
120 ft-lb/in²
ASTM D1822
ExxonMobil Paxon™ BC50-100 Sheet Extrusion and Blow Molding Resin  (discontinued **)
BC50-100 is a high molecular weight, high density polyethylene copolymer. This resin has superior stress crack resistance, high impact strength and good rigidity.Information provided by ExxonMobil ..