ExxonMobil HDPE HD 9856B High Density Polyethylene Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Exxon Chemical
Trade Name HDPE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil HDPE HD 9856B High Density Polyethylene Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: HD 9856B is a HDPE blow molding resin designed for high performance packaging applications. Containers made from HD 9856B exhibit a unique combination of stiffness and environmental stress cracking resistance. These properties, coupled with excellent processability on both continuous and intermittent equipment, afford significant lightweighting and/or fast-cycling potential in many applications. HD 9856B does not contain any antistatic.Availability: Latin America, North America and South America Additive: Thermal Stabilizer: YesAntistatic: NoUV Stabilizer: NoApplications: Caps and ClosuresCompression MoldingsFood packagingHousehold and Industrial chemical containersPharmaceutical PackagingThermoformed PartsThin Gauge SheetInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.957 g/cc
0.0346 lb/in³
ASTM D4883
ESCR 100% Igepal® >= 1000 hour
>= 1000 hour
F50; ASTM D1963A
Melt Flow 0.46 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.46 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 30.3 MPa
4400 psi
ASTM D638
Elongation at Break 1100 %
1100 %
ASTM D638
Flexural Modulus 1.45 GPa
210 ksi
ASTM D790B
Flexural Modulus, 1% Secant 1450 MPa
210000 psi
ASTM D790A
Tensile Impact Strength 252 kJ/m²
120 ft-lb/in²
ASTM D1822
Thermal Properties Metric English Comments
Brittleness Temperature <= -76.1 °C
<= -105 °F
ASTM D746